상세 보기
초록
In original publication, Table 1 contains errors. The corrected Table 1 is presented below: (Table presented.) Table 1 Parameter Unit QWR HWR Frequency MHz 81.25 162.5 βOPT 0.051 0.13 Leff mm 186.5 236.3 Q0 109 0.24 2.3 QRs Ω 18.1 37.1 R/Q Ω 474 298 Eacc MV/m 6.1 6.6 Epeak/Eacc 6.0 5.5 Bpeak/Eacc mT/(MV/m) 10.8 9.6 According to the corrected Table 1, the following textual corrections should be noted: The effective lengths (Leff) for the QWR and HWR superconducting cavities are 186.5 and 236.3 mm, respectively, and their Epeak/Eacc ratios are 6.0 and 5.5, respectively. The Bpeak/Eacc ratios for the two cavities are 10.8 and 9.6 mT/(MV/m), respectively, and the required quality factor for the QWR cavities should be higher than 2.4 × 108 at 6.1 MV/m and 4.5 K. The required quality factor for the HWR cavities should be higher than 2.3 × 109 at 6.6 MV/m and 2.05 K. © The Korean Physical Society 2025.
- 제목
- Superconducting cavities for SCL3 (DEC, 10.1007/s40042-024-01267-5, 2024)
- 저자
- Kim, Heetae; Jeon, Sungmin; Kim, Juwan; Lee, Junwoo; Kim, Moosang; Joo, Jongdae; Hyun, Myung Ook; Jung, Hoe Chun; Jang, Hyojae; Kim, Youngkwon; Park, Gunn-Tae; Joung, Mijoung; Jung, Yoochul
- 발행일
- 2025-09
- 유형
- Correction
- 권
- 87
- 호
- 5
- 페이지
- 727 ~ 727
- 언어
- ENG
- 출판사
- KOREAN PHYSICAL SOC
- 발행국가
- 대한민국
- 분량
- 1 페이지
- ISSN
- E 1976-8524