Extrusion limit diagram of AZ91-0.9Ca-0.6Y-0.5MM alloy and effects of extrusion parameters on its microstructure and mechanical properties

  • Lee, Dong Hee; 
  • Kim, Ye Jin; 
  • Kim, Sang-Hoon; 
  • Moon, Byoung Gi; 
  • Park, Sung Hyuk
Citations

WEB OF SCIENCE

27
Citations

SCOPUS

30

초록

An AZ91-0.9Ca-0.6Y-0.5MM (AZXWMM91100) alloy, which has higher corrosion resistance, ignition resistance, and extrudability than a commercial AZ91 alloy, has been developed recently. In this study, the AZXWMM91100 alloy is extruded at various temperatures (300-400 degrees C) and ram speeds (1-14.5 mm/s), and the cracking behaviors, microstructure, and tensile properties of the extruded materials are systematically analyzed. On the basis of the pressure limit and surface and internal cracking limit, the extrusion limit diagram providing a safe extrusion processing zone is established. All of the materials extruded at temperatures and speeds within the safe extrusion processing zone have high surface quality and moderate tensile ductility with an elongation higher than 10%. Moreover, they have a fully recrystallized grain structure and contain undissolved particle stringers arranged parallel to the extrusion direction. The grain size of the extruded material does not show any relationship with the Zener-Hollomon parameter (Z). However, the yield strength (YS) of the extruded material is inversely proportional to the logarithm of the Z value, and their relationship is expressed as YS = -31.2(center dot)log(Z) + 536. These findings may broaden the understanding of the AZXWMM91100 alloy with excellent chemical and physical properties and provide valuable information for the development of high-performance extruded Mg products using this alloy. (c) 2021 Chongqing University. Publishing services provided by Elsevier B.V. on behalf of KeAi Communications Co. Ltd. This is an open access article under the CC BY-NC-ND license (http://creativecommons.org/licenses/by-nc-nd/4.0/) Peer review under responsibility of Chongqing University

키워드

Magnesium; Extrudability; Extrusion limit diagram; Microstructure; Tensile properties; GRAIN-REFINEMENT; HOT DEFORMATION; FLOW-STRESS; MG ALLOY; MAGNESIUM; TEMPERATURE; STRENGTH; BEHAVIOR; CA; SPEED
제목
Extrusion limit diagram of AZ91-0.9Ca-0.6Y-0.5MM alloy and effects of extrusion parameters on its microstructure and mechanical properties
저자
Lee, Dong Hee; Kim, Ye Jin; Kim, Sang-Hoon; Moon, Byoung Gi; Park, Sung Hyuk
DOI
10.1016/j.jma.2021.06.002
발행일
2022-12
유형
Article
저널명
Journal of Magnesium and Alloys
권
10
호
12
페이지
3447 ~ 3458